Experimental research on utilization of coal gangue as clay for optimized formula on cement clinker calcination
QIU Guo-hua, SHI Zheng-lun, YU Chun-jiang,XU Yang, QIU kun-zan,SHI Zheng-zhan, LUO Zhong-yang
(State Key Laboratory of Clean Energy Utilization, Zhejiang University, Hangzhou 310027, China)
Download:   PDF(0KB) HTML
Export: BibTeX | EndNote (RIS)      

Abstract  

Six kinds of cement raw material were matched to use different coal gangues and different limestones in order to obtain the calcine thermal condition and the reasonable prescription of the gangue instead of clay ingredient which was applied to the cement production. Experiments were conducted under different temperatures in the laboratory chamotte calcine test platform. For the samples of the calcined cement clinker, their mass fractions of free-CaO were measured, and their mineral components were qualitatively analyzed by X-ray diffraction (XRD). Results show that qualified cement clinker can be generated by the utilization of coal gangue instead of clay mixed with middle-calcium limestone, high and middle-calcium limestone; the calcinations temperature are at least lower 50 ℃ than that of clay ingredients, while the high-calcium limestone has no obvious change. A high grade cement clinker can be calcined by mixing the coal gangue with middle-calcium limestone or high and middle-calcium limestone.



Published: 09 March 2010
CLC:  TQ 172.4  
Cite this article:

QIU Guo-Hua, SHI Zheng-Lun, TU Chun-Jiang, et al. Experimental research on utilization of coal gangue as clay for optimized formula on cement clinker calcination. J4, 2010, 44(2): 315-319.

URL:

http://www.zjujournals.com/eng/10.3785/j.issn.1008-973X.2010.02.019     OR     http://www.zjujournals.com/eng/Y2010/V44/I2/315


煤矸石代黏土煅烧水泥熟料配方优化试验研究

为获得煤矸石代黏土配料应用于水泥生产的煅烧热工条件和合理配方,选取不同煤矸石和不同品位的石灰石等原料配制6种水泥生料,在实验室熟料煅烧试验台中进行不同温度下煅烧水泥熟料的试验研究,对试验所得的熟料样品分别进行了游离CaO质量分数的测定和矿物组成的X射线衍射(XRD)分析.试验结果表明:煤矸石代黏土与中钙石灰石和高中钙石灰石配料,都能烧制出合格的水泥熟料,烧成温度比黏土配料的烧成温度降低50 ℃以上;而煤矸石与高钙石灰石的配方则在烧成温度上没有明显优势,说明煤矸石与中钙石灰石或高中钙石灰石配料更能烧制出高质量的水泥熟料.

[1] 潘淑琴,王中伟. 煤矸石部分代替粘土生产水泥的实践[J]. 新世纪水泥导报,2004(增刊): 113114.
PAN Shu-qin, WANG Zhong-wei. The practice of the coal gangue part replaces the clay production cement[J]. New Century Cement Review, 2004(supplement): 113114.
[2] 孙星寿,周贺.国内外水泥行业对比研究及政策思考[J].中国水泥,2002(7): 6467.
SUN Xing-shou, ZHOU-he. Contrast research and policy ponder of domestic and foreign cement profession[J]. Chinese Cement, 2002(7): 6467.
[3] 国家统计局.中国统计年鉴[M].北京:中国统计出版社,2006: 24.
[4] 张忠伦,隋同波,丁洪涛,等.煤矸石在水泥工业的应用研究[C]//智能与绿色建筑文集.北京:中国建筑工业出版社,2006: 7882.
ZHANG Zhong-lun, SUI tong-bo, DING hong-tao, et al. Applied research on coal gangue in cement industry[C]// The Anthology of Intelligent and Green Construction. Beijing: China Building Industry Publishing Press, 2006: 7882.
[5] 边炳鑫,解强,赵由才.煤系固体废弃物资源化技术[M].北京:化学工业出版社,2005: 63.
[6]王拈生,傅圣勇.水泥新原料烧成新技术与新论[M].北京:中国科学技术出版社,1999: 5660.
[7] ALI M M, AQARWAL S K, MOHAN K. Making use of limestone[J]. World Cement, 2005, 36(6): 8791.

[1] QIU Guo-Hua, XU Yang, SHI Zheng-Lun, FANG Meng-Xiang, JIA Zhong-Yang, CEN Ge-Fa. Feasibility analysis on utilization of coal gangue as clay for cement[J]. J4, 2010, 44(5): 1003-1008.