机械与能源工程 |
|
|
|
|
应变强化奥氏体不锈钢焊接接头冲击试验研究 |
舒翔宇1,郑津洋1,寿比南2,缪存坚1,黄泽1,郭阿宾1 |
1.浙江大学 化工机械研究所, 浙江 杭州 310027; 2. 全国压力容器标准化委员会,北京 100029 |
|
Experimental study on impact behavior of austenitic stainless
steel welding joints after cold stretching |
SHU Xiang-yu1, ZHENG Jin-yang1, SHOU Bi-nan2, MIAO Cun-jian1,
HUANG Ze1, GUO A-bin1 |
1. Institute of Chemical Machinery and Process Equipment, Zhejiang University, Hangzhou 310027, China;
2. China Standardization Committee on Boilers and Pressure Vessels, Beijing 100029, China |
引用本文:
舒翔宇,郑津洋,寿比南,缪存坚,黄泽,郭阿宾. 应变强化奥氏体不锈钢焊接接头冲击试验研究[J]. J4, 2012, 46(7): 1162-1167.
SHU Xiang-yu, ZHENG Jin-yang, SHOU Bi-nan, MIAO Cun-jian, HUANG Ze, GUO A-bin. Experimental study on impact behavior of austenitic stainless
steel welding joints after cold stretching. J4, 2012, 46(7): 1162-1167.
链接本文:
http://www.zjujournals.com/eng/CN/10.3785/j.issn.1008-973X.2012.07.002
或
http://www.zjujournals.com/eng/CN/Y2012/V46/I7/1162
|
[1] 郑津洋, 郭阿宾, 缪存坚, 等. 奥氏体不锈钢深冷容器室温应变强化技术[J]. 压力容器, 2010, 27(8): 28-56.
ZHENG Jinyang, GUO Abin, MIAO Cunjian, et al. Cold stretching technique for austenitic stainless steel cryogenic pressure vessels [J].Pressure Vessel Technology, 2010, 27(8): 28-56.
[2] BRAUTIGAM M, HARING H W, KOPL H. Pressure vessels for cryogenic service: some new aspects of materials and construction [C]∥The 7th International Conference on Pressure Vessel Technology. Dusseldorf: [s. n.], 1992: 887-899.
[3] SREENIVASAN P R. Charpy energylateral expansion relations for a wide range of steels [J]. International Journal of Pressure Vessels and Piping, 2006, 83(7): 498-504.
[4] GB 24511, 承压设备用不锈钢钢板及钢带[S].北京:中国标准出版社, 2009.
[5] GB/T 20878, 不锈钢耐热钢牌号及化学成分[S].北京:中国标准出版社, 2007.
[6] GB 150, 压力容器[S].北京:中国标准出版社, 2011.
[7] ASME Boiler and Pressure Vessel Code Ⅷ Division 1:, Rules for construction of pressure vessels [S]. New York: ASME, 2010.
[8] ASME Boiler and Pressure Vessel Code Ⅷ Division 2:, Alternative rules: rules for construction of pressure vessels [S]. New York: ASME, 2010.
[9] EN 13445, Unfired pressure vessels[S]. Brussels: European Committee for Standardization, 2009.
[10] GB/T 2650, 焊接接头冲击试验方法[S].北京:中国标准出版社, 2008.
[11] GB/T 229, 金属材料夏比摆锤冲击试验方法[S].北京:中国标准出版社, 2007.
[12] NB/T 47016, 承压设备产品焊接试件的力学性能检验[S]. 北京:新华出版社, 2011.
[13] JIS B8266, Alternative standard for construction of pressure vessels [S]. Tokyo: JISC, 2003.
[14] JIS G3460, Steel pipes for low temperature service [S]. Tokyo: JISC, 2006.
[15] TOWERS O L. Testing of subsized Charpy specimens. Part 2: the influence of specimen thickness on upper shelf behavior [J]. Metal Construction, 1986, 18(4): 254R-258R.
[16] KRAFFT J M, SULLIVAN A M, BOYLE R W. Effect of dimensions on fast fracture instability of notched sheets [C]∥ Proceedings of the Crack Propagation Symposium. Cranfield: [s. n.], 1961: 8-28.
[17] WALLIN K. Upper shelf energy normalization for subsized CharpyV specimens [J]. International Journal of Pressure Vessels and Piping, 2001, 78(7): 463-470.
[18] TOWERS O L. Testing of subsized Charpy specimens. Part 1: the influence of specimen thickness on the ductile/brittle transition [J]. Metal Construction, 1986, 18(3): 171R-176R.
[19] BRAMFITT B L, MARDER A R. A study of the delamination behavior of a very lowcarbon steel [J]. Metallurgical Transaction A, 1977, 8A: 1263-1273. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|