工程设计学报  2001, Vol. 8 Issue (2): 69-72    
工程设计理论、方法与技术     
表面裂纹应力强度因子计算及扩展跟踪的权函数法
 梁文军1, 金志江2
1.杭州市锅炉压力容器检验研究所,浙江杭州310005;
 2.浙江大学化工机械研究所,浙江杭州310027
Weight Function Method of Evaluating SIF and Tracing the Development of Surface Crack
 LIANG  Wen-Jun1, JIN  Zhi-Jiang2
1.Hangzhou Boiler &Pressure Vessel Inspection Institute, Hangzhou 31005, China;
2.Research Institute of Chemical Machinery and Equipment, Zhejiang University, Hangzhou 310027, China
 全文: PDF(135 KB)   HTML
摘要: 介绍了一种显式的权函数法,并将这种方法用于圆柱形容器接管外拐角表面裂纹的应力强度因子计算和扩展跟踪上.结果表明,权函数法可以用于分析各种载荷下不同形状的裂纹.就一般的工程问题而言,权函数法不失为一种与有限元法互补的方便有效的分析方法.
关键词: 表面裂纹应力强度因子权函数    
Abstract:  An overall introduction of a new method of evaluating SIF—Weight Function is given. This is used to trace the development of the surface crack in the nozzle' s out-corner. It can beobserved that WF can be used to analyze the surface crack of various shapes under various load. For general engineering questions, WF is fairly accurate and a good substitute of FEM.
Key words:  surface crack    stress intensity factor(SIF)    weight function(WF)
出版日期: 2001-06-15
基金资助:

浙江省自然科学基金资助项目(599093)

服务  
把本文推荐给朋友
加入引用管理器
E-mail Alert
RSS
作者相关文章  
梁文军
金志江

引用本文:

梁文军, 金志江. 表面裂纹应力强度因子计算及扩展跟踪的权函数法[J]. 工程设计学报, 2001, 8(2): 69-72.

LIANG Wen-Jun, JIN Zhi-Jiang. Weight Function Method of Evaluating SIF and Tracing the Development of Surface Crack[J]. Chinese Journal of Engineering Design, 2001, 8(2): 69-72.

链接本文:

https://www.zjujournals.com/gcsjxb/CN/        https://www.zjujournals.com/gcsjxb/CN/Y2001/V8/I2/69

[1] 任远, 张成成, 高靖云, 李孟光. 涡轮盘篦齿裂纹扩展的有限元数值模拟[J]. 工程设计学报, 2016, 23(2): 152-159,165.
[2] 何家胜,朱光强,朱晓明,路远明,吴建平. 弯扭组合载荷下圆管半椭圆表面裂纹应力强度因子的有限元分析[J]. 工程设计学报, 2007, 14(2): 153-159.
[3] 金志江. 圆筒型容器接管外拐角表面裂纹疲劳扩展的有限元跟踪[J]. 工程设计学报, 2000, 7(1): 42-45.