表 4 电池各向异性热导率校准值
Tab.4 Calibrated anisotropic thermal conductivity of battery
W/(m·K)
方向$\theta $/℃新电池鼓包电池
测试平均值校准值测试平均值校准值
厚度−202.662.56——
厚度02.582.48——
厚度202.662.562.232.14
厚度402.702.59——
宽度208.257.937.607.30
高度208.127.807.417.11