石灰激发低碳胶凝材料的水化特性与力学性能 |
| 吴萌,张云升,刘志勇,刘诚,佘伟,王立国,马瑞 |
|
Hydration characteristics and mechanical performance of lime and gypsum-activated low carbon cementitious materials |
| Meng WU,Yunsheng ZHANG,Zhiyong LIU,Cheng LIU,Wei SHE,Liguo WANG,Rui MA |
| 图 6 水化90 d时LCM样品的MIP试验测试结果 |
| Fig.6 Result of MIP test of LCM samples at 90 days |
|