石灰激发低碳胶凝材料的水化特性与力学性能
吴萌,张云升,刘志勇,刘诚,佘伟,王立国,马瑞

Hydration characteristics and mechanical performance of lime and gypsum-activated low carbon cementitious materials
Meng WU,Yunsheng ZHANG,Zhiyong LIU,Cheng LIU,Wei SHE,Liguo WANG,Rui MA
表 3 LCM各样品的氢氧化钙与化学结合水质量分数
Tab.3 Content of Ca(OH)2 and chemically bound water in LCM samples at 90 days
样品wB/%
氢氧化钙(TGA)氢氧化钙(QXRD)化学结合水
C1-90 d3.93.713.8
C2-90 d4.24.113.5
C3-90 d6.56.714.7
C4-90 d10.811.715.4
C5-90 d9.710.315.7