表 5 试件的高温后试验结果 |
Tab.5 Post-fire test result of specimens |
|
试件编号 | θ/℃ | μ | Fμ/kN | 破坏阶段 | 破坏模式 | FY,R/kN | FY,R/FY | FU,R/kN | FU,R/FU | S1 | 500 | 0.25 | 7.1 | 阶段3 | 钢管屈服破坏 | 27.0 | 0.96 | 39.7 | 0.95 | S1 | 500 | 0.50 | 14.1 | 阶段3 | 钢管屈服破坏 | 26.8 | 0.95 | 38.8 | 0.93 | S1 | 700 | 0.25 | 7.1 | 阶段2 | 钢管屈服破坏 | — | — | — | — | S2 | 500 | 0.25 | 29.7 | 阶段3 | 端板屈服伴随螺栓破坏 | 107.6 | 0.91 | 164.9 | 0.95 | S2 | 500 | 0.50 | 59.4 | 阶段3 | 端板屈服伴随螺栓破坏 | 104.3 | 0.88 | 153.7 | 0.89 | S2 | 700 | 0.25 | 29.7 | 阶段2 | 端板屈服伴随螺栓破坏 | — | — | — | — | S3 | 500 | 0.25 | 12.0 | 阶段3 | 端板屈服破坏 | 44.1 | 0.92 | 62.1 | 0.88 | S3 | 500 | 0.50 | 23.9 | 阶段3 | 端板屈服破坏 | 43.4 | 0.91 | 61.9 | 0.88 | S3 | 700 | 0.25 | 12.0 | 阶段3 | 端板屈服破坏 | 43.1 | 0.91 | 62.7 | 0.89 | S4 | 500 | 0.25 | 18.6 | 阶段3 | 螺栓拉断 | 70.2 | 0.95 | 91.1 | 0.98 | S4 | 500 | 0.50 | 37.1 | 阶段3 | 螺栓拉断 | 69.3 | 0.94 | 89.7 | 0.96 | S4 | 700 | 0.25 | 18.6 | 阶段2 | 螺栓拉断 | — | — | — | — | S5 | 500 | 0.25 | 7.3 | 阶段3 | 钢管屈服破坏 | 27.1 | 0.93 | 48.8 | 0.94 | S5 | 500 | 0.50 | 14.6 | 阶段3 | 钢管屈服破坏 | 26.8 | 0.92 | 48.7 | 0.93 | S5 | 700 | 0.25 | 7.3 | 阶段3 | 钢管屈服破坏 | 26.3 | 0.90 | 48.8 | 0.94 | S6 | 500 | 0.25 | 30.1 | 阶段3 | 端板屈服伴随螺栓破坏 | 114.3 | 0.95 | 180.4 | 0.97 | S6 | 500 | 0.50 | 60.1 | 阶段3 | 端板屈服伴随螺栓破坏 | 113.2 | 0.94 | 174.7 | 0.94 | S6 | 700 | 0.25 | 30.1 | 阶段3 | 端板屈服伴随螺栓破坏 | — | — | — | — |
|
|
|