熔融沉积成型3D打印拉丝缺陷的正交实验研究
|
|
白永健,陈赟,张思,陈康,苏世杰
|
Orthogonal experiment of fused deposition molding 3D printing drawing defects
|
|
Yong-jian BAI,Yun CHEN,Si ZHANG,Kang CHEN,Shi-jie SU
|
|
| 表 5 峭度指标方差分析 |
| Tab.5 Analysis of variance of kurtosis index |
|
| 指标 | 方差来源 | df | SS | MS | F | | 传感器Ⅰ峭度 | A | 2 | 8.53 | 4.27 | 5.47 | | B | 2 | 5.00 | 2.50 | 3.21 | | C | 2 | 17.34 | 8.67 | 11.13 | | D | 2 | 1.85 | 0.93 | 1.19 | | 传感器Ⅱ峭度 | A | 2 | 9.94 | 4.97 | 7.42 | | B | 2 | 5.88 | 2.94 | 4.39 | | C | 2 | 7.49 | 3.75 | 5.59 | | D | 2 | 5.01 | 2.51 | 3.74 | | 传感器Ⅲ峭度 | A | 2 | 5.56 | 2.78 | 4.09 | | B | 2 | 1.03 | 0.52 | 0.76 | | C | 2 | 26.59 | 13.29 | 19.59 | | D | 2 | 2.05 | 1.02 | 1.51 |
|
|
|