高渗透压-硫酸盐侵蚀下混凝土时空劣化 |
李睿鑫,邹贻权,胡大伟,周辉,王冲,周永祥,王祖琦 |
Spatiotemporal deterioration of concrete under high osmotic pressure and sulfate attack |
Rui-xin LI,Yi-quan ZOU,Da-wei HU,Hui ZHOU,Chong WANG,Yong-xiang ZHOU,Zu-qi WANG |
图 20 不同渗透压下8、6、4、2和0 mm侵蚀深度处CT切片 |
Fig.20 CT section pictures at 8,6,4,2 and 0 mm erosion depth under different osmotic pressure were taken in turn |
![]() |