表 3 天然骨料混凝土配合比
Tab.3 Mixing ratio of natural aggregate concrete
混凝土编号 mw /kg mc /kg m4 /kg m5 /kg ma /kg S /mm fcu,28 /MPa 强度评级
N-C25 172.4 252.0 988.1 988.1 2.520 150 28.8 C25
N-C30 161.2 280.5 990.9 990.9 2.805 170 36.0 C30
N-C35 150.0 302.7 996.5 996.5 3.207 160 41.1 C35