PC/ABS合金的气相/凝聚相协同阻燃作用
|
高顺,郭正虹
|
Synergistic flame retardancy of gas phase and condensed phase of PC/ABS alloy
|
Shun GAO,Zheng-hong GUO
|
|
表 1 阻燃PC/ABS合金配比表 |
Tab.1 Formulations of flame retardant PC/ABS alloy |
|
组成 | wB /% | PC | ABS | RDP | TPP | PTFE1) | MBS | 1)注:PTFE作为抗滴落剂存在,每组配方都是相同份数 | PC/ABS | 70.0 | 30.0 | − | − | − | − | PC/ABS/10TPP | 62.7 | 26.9 | − | 10 | 0.4 | − | PC/ABS/10RDP | 62.7 | 26.9 | 10 | − | 0.4 | − | PC/ABS/(8RDP+2TPP) | 62.7 | 26.9 | 8 | 2 | 0.4 | − | PC/ABS/(6RDP+4TPP) | 62.7 | 26.9 | 6 | 4 | 0.4 | − | PC/ABS/(5RDP+5TPP) | 62.7 | 26.9 | 5 | 5 | 0.4 | − | PC/ABS/(4RDP+6TPP) | 62.7 | 26.9 | 4 | 6 | 0.4 | − | PC/ABS/(2RDP+8TPP) | 62.7 | 26.9 | 2 | 8 | 0.4 | − | PC/ABS/(6RDP+4TPP)/5MBS | 59.2 | 25.4 | 6 | 4 | 0.4 | 5 | PC/ABS/(6RDP+4TPP)/10MBS | 55.7 | 23.9 | 6 | 4 | 0.4 | 10 | PC/ABS/(6RDP+4TPP)/15MBS | 52.2 | 22.4 | 6 | 4 | 0.4 | 15 |
|
|
|