重塑高岭土渗透各向异性影响因素
余良贵,周建,温晓贵,徐杰,罗凌晖

Factors influencing permeability anisotropy of remolded kaolin
Liang-gui YU,Jian ZHOU,Xiao-gui WEN,Jie XU,Ling-hui LUO
表 5 不同溶液下制取的重塑高岭土液塑限
Tab.5 Liquid and plastic limits of remolded kaolin prepared with different solutions
溶液类型 0.01 mol/L 0.10 mol/L
ωL ωP ωL ωP
超纯水 65.35 40.04 65.35 40.04
氯化钠 63.99 42.61 59.67 40.25
氯化钾 63.36 42.36 59.22 40.33
氯化钙 63.12 41.03 58.89 40.18