摘要:

为研究多铁性复合材料中界面特性对磁电耦合的影响,建立一种采用界面内聚力单元的多铁性复合材料有限元分析模型.基于压电和压磁材料本构关系的模拟特性,采用压电有限单元模拟各单相材料;将内聚力模型用于表征界面上相间相互作用力和位移间断之间的关系,可描述非理想界面的刚度和强度,并通过相应的内聚力单元来实现.各种非理想界面状况可通过调节内聚力模型参数来表征,而理想界面可通过对界面刚度加强来模拟.具有理想界面的层状多铁性复合材料的算例分析结果与文献一致.采用本文的有限元模型分析了非理想界面的刚度对磁电耦合的影响,计算了相应的磁电耦合系数.结果表明,界面刚度对复合材料的磁电系数有重要影响,当界面刚度足够大时,界面特性接近于理想界面,磁电系数趋于恒定.本文方法和结果对理论和实际中界面处理、磁电耦合性能的预测具有参考意义.

Abstract:

In order to study the influences of interfaces on magnetoelectric (ME) coupling, a finite element model for multiferroics composites was suggested by employing cohesive zone elements for the interfaces. Piezoelectric elements were utilized for both piezoelectric and piezomagnetic phases based on the analogy between piezoelectric and piezomagnetic constitutive relations. And cohesive zone models (CZM) were employed to represent the relation between tractions and displacement discontinuities on imperfect interfaces, which characterized the stiffness and toughness of interfaces and were implemented by cohesive zone elements. Imperfect interfaces can be modeled by adopting CZM parameters, and perfect interfaces are also possible to be approximately modeled by CZM with enhanced interfacial stiffness. Example results of laminated multiferroics composites with ideal interfaces show good agreement with those in literature. The influences of imperfect interfaces on ME coupling were analyzed by the present finite element model, the corresponding ME coefficients were calculated. The simulation results indicate that the interface stiffness plays a significant role on ME coefficient of the composites. When the interfaces are stiff enough, they tend to be perfect and the ME coefficient tends to a constant. The present method and results are of reference significance to process of interfacial bonding and prediction of ME properties.

出版日期: 2012-05-01
:  O 34  
基金资助:

国家自然科学基金资助项目(10832009, 10972194);浙江省自然科学基金资助项目(Y7080297).

通讯作者: 陶伟明,男,博导, 教授.     E-mail: taowm@zju.edu.cn
作者简介: 钱治宏(1988-),男,硕士生,主要从事多场耦合力学和复杂结构力学分析. E-mail: zhihong523@yahoo.com.cn
服务  
把本文推荐给朋友
加入引用管理器
E-mail Alert
RSS
作者相关文章  

引用本文:

钱治宏, 陶伟明, 杨兴旺. 多铁性复合材料非理想界面的模拟及其影响[J]. J4, 2012, 46(5): 935-940.

QIAN Zhi-hong, TAO Wei-ming, YANG Xing-wang. Modeling and influences of imperfect interfaces
in multiferroic composites. J4, 2012, 46(5): 935-940.

链接本文:

http://www.zjujournals.com/eng/CN/10.3785/j.issn.1008-973X.2012.05.026        http://www.zjujournals.com/eng/CN/Y2012/V46/I5/935

[1] EERENSTEIN W, MATHUR N D, SCOTT J F. Multiferroic and magnetoelectric materials[J]. Nature, 2006, 442(7104): 759-765.
[2] YUAN Guoliang, OR S W. Multiferroicity in polarized singlephaseBi0.875Sm0.125FeO3ceramics[J]. Journal of Applied Physics , 2006 , 100(2): 024109.
[3] YUAN Guoliang, OR SW, LIU Junming, et al. Structural transformation and ferroelectromagnetic behavior in singlephaseBi1xNdxFeO3multiferroic ceramics [J]. Applied Physics Letters, 2006, 89(5): 052905.
[4] WANG Yiping, YUAN Guoliang, CHEN Xiaoyuan, et al. Electrical and magnetic properties of singlephased and highly resistive ferroelectromagnet BiFeO3ceramic[J]. Journal of Physics D: Applied Physics, 2006, 39(10): 2019-2023.
[5] SPALDIN N A, FIEBIG M. The renaissance of magnetoelectric multiferroics [J]. Science, 2005, 309(5733): 391-392.
[6] NAN Cewen. Magnetoelectric effect in composites of piezoelectric and piezomagnetic phases [J]. Physical Review B, 1994(50): 6082-6088.
[7] PAN E, WANG R. Effects of geometric size and mechanical boundary conditions on magnetoelectric coupling in multiferroic composites [J]. Journal of Physics D:Applied Physics, 2009, 42(24):245503.
[8] NAN Cewen, BICHURIN M I, DONG Shuxiang, et al. Multiferroic magnetoelectric composites: Historical perspective, status, and future directions [J]. Journal of Applied Physics, 2008, 103: 031101.
[9] NEEDLEMAN A. A continuum model for void nucleation by inclusion debonding [J]. Journal of Applied Mechanics Transactions of The Asme, 1987, 54(3): 525-531.
[10] NEEDLEMAN A. An analysis of tensile decohesion along an interface [J]. Journal of The Mechanics and Physics of Solids, 1990, 38(3): 289-324.
[11] CAMACHO G T, ORTIZ M. Computational modeling of impact damage in brittle materials [J]. International Journal of Solids and Structures,1996,33(20/22): 2899-2938.
[12] GEUBELLE P H, BAYLOR J . Impactinduced delamination of laminated composites: A 2D simulation [J]. Composites Part BEngineering, 1998, 29: 589-602.
[13] 闫亚宾, 尚福林. PZT薄膜界面分层破坏的内聚力模拟[J]. 中国科学, 2009, 39(7): 1007-1017.
YAN Yabin, SHANG Fulin. Choesive zone modeling of interfacial delamination in PZT thin films [J]. Science in China, 2009, 39(7): 1007-1017.
[14] 曲凯, 张旭东, 李高春. 基于内聚力界面脱黏的复合固体推进剂力学性能研究[J], 火炸药学报, 2008, 31(6): 77-81.
QU Kai, ZHANG Xudong, LI Gaochun. Research on mechanical performance of composite propellant with cohesive interface debonding [J]. Chinese Journal of Explosives and Propellants, 2008, 31(6): 77-81.
[15] 周储伟,杨卫,方岱宁. 内聚力界面单元与复合材料的界面损伤分析[J]. 力学学报,1999,31(3): 372-377.
ZHOU Chuwei, YANG Wei, FANG Daining. Cohesive interface element and interfacial damage analysis of composites [J]. Acta Mechanica Sinica, 1999, 31(3): 372-377.
[16] BLACKBURN J F, VOPSAROIU M, CAIN M G. Verified finite element simulation of multiferroic structures: Solutions for conducting and insulating systems [J]. Journal of Applied Physics, 2008, 104: 074104.

[1] 李正伟, 陶伟明. 非共面薄膜-基底结构多层封装及延展性分析[J]. J4, 2012, 46(6): 1143-1147.
[2] 李莹,殷中科,曹晓,邓水光. 增强JavaCard中Schnorr签名的预处理方案[J]. J4, 2012, 46(3): 386-391.
[3] 王惠明,赵志城. 界面缺陷对压电薄层复合结构中Love波的影响[J]. J4, 2012, 46(3): 555-559.
[4] 凌道盛, 卜令方, 黄根清, 黄博. 平面强化有限单元法的h型网格自适应[J]. J4, 2011, 45(12): 2150-2158.
[5] 陈小安,邵冰莓,宋顺成,王庭辉. 高氮合金钢高应变率剪切性能测试[J]. J4, 2011, 45(11): 1948-1952.
[6] 刘承斌, 边祖光, 陈伟球. 叠层压电球壳的三维热释电分析[J]. J4, 2011, 45(6): 1067-1073.
[7] 高洪伟, 何丽莎, 张永强. 考虑尺寸效应的厚壁圆筒统一塑性极限解[J]. J4, 2011, 45(4): 684-687.
[8] 施彦彬,何闻,郑建毅. Q235钢应变释放系数塑性修正问题的研究[J]. J4, 2010, 44(11): 2083-2087.
[9] 蒋军, 徐正红, 徐凌峰. 颗粒体材料中的力链压曲变形[J]. J4, 2010, 44(10): 1931-1937.
[10] 陈伟梁, 徐博侯, 黄磊. 大型汽轮发电机定子绕组端部的振动分析[J]. J4, 2010, 44(8): 1558-1561.
[11] 杨兴旺, 毕国丽, 张雪, 等. 激光控制裂纹扩展的路径迭代法及收敛性分析[J]. J4, 2009, 43(11): 2043-2047.